G80 Grade Load Steel Lifting Hege Prestaasjeketting 12mm
G80 Grade Load Steel Lifting Hege Prestaasjeketting 12mm
Kategory
Oanfraach
Relatearre produkten
Kettingparameter
SCIC Grade 80 (G80) keatlingen foar it heffen binne makke neffens EN 818-2 noarmen, mei nikkel-chroom-molybdeen-mangaanlegearing stiel neffens DIN 17115 noarmen; goed ûntworpen / kontroleare lassen en waarmtebehanneling soargje foar meganyske eigenskippen fan keatlingen, ynklusyf testkrêft, brekkrêft, ferlinging en hurdens.
Figuer 1: Ofmjittings fan kettingferbining fan klasse 80
tabel 1: Grade 80 (G80) chain dimensions, EN 818-2
| diameter | toanhichte | breedte | gewicht fan 'e ienheid | |||
| nominaal | tolerânsje | p (mm) | tolerânsje | binnenste W1 | bûtenste W2 | |
| 6 | ± 0,24 | 18 | ± 0,5 | 7.8 | 22.2 | 0.8 |
| 7 | ± 0,28 | 21 | ± 0,6 | 9.1 | 25.9 | 1.1 |
| 8 | ± 0,32 | 24 | ± 0,7 | 10.4 | 29.6 | 1.4 |
| 10 | ± 0,4 | 30 | ± 0,9 | 13 | 37 | 2.2 |
| 13 | ± 0,52 | 39 | ± 1.2 | 16.9 | 48.1 | 4.1 |
| 16 | ± 0,64 | 48 | ± 1.4 | 20.8 | 59.2 | 6.2 |
| 18 | ± 0,9 | 54 | ± 1.6 | 23.4 | 66.6 | 8 |
| 19 | ± 1 | 57 | ± 1.7 | 24.7 | 70.3 | 9 |
| 20 | ± 1 | 60 | ± 1.8 | 26 | 74 | 9.9 |
| 22 | ± 1.1 | 66 | ± 2.0 | 28.6 | 81.4 | 12 |
| 23 | ± 1.2 | 69 | ± 2.1 | 29.9 | 85.1 | 13.1 |
| 24 | ± 1.2 | 72 | ± 2.1 | 30 | 84 | 14.5 |
| 25 | ± 1.3 | 75 | ± 2.2 | 32.5 | 92.5 | 15.6 |
| 26 | ± 1.3 | 78 | ± 2.3 | 33.8 | 96.2 | 16.8 |
| 28 | ± 1.4 | 84 | ± 2,5 | 36.4 | 104 | 19.5 |
| 30 | ± 1.5 | 90 | ± 2,7 | 37.5 | 105 | 22.1 |
| 32 | ± 1.6 | 96 | ± 2,9 | 41.6 | 118 | 25.4 |
| 36 | ± 1.8 | 108 | ± 3.2 | 46.8 | 133 | 32.1 |
| 38 | ± 1.9 | 114 | ± 3.4 | 49.4 | 140.6 | 35.8 |
| 40 | ± 2 | 120 | ± 4.0 | 52 | 148 | 39.7 |
| 45 | ± 2.3 | 135 | ± 4.0 | 58.5 | 167 | 52.2 |
| 48 | ± 2.4 | 144 | ± 4.3 | 62.4 | 177.6 | 57.2 |
| 50 | ± 2.6 | 150 | ± 4,5 | 65 | 185 | 62 |
Tabel 2: Mechanyske eigenskippen fan ketting fan klasse 80 (G80), EN 818-2
| diameter | wurklastlimyt | produksjebewiiskrêft | min. brekkrêft |
| 6 | 1.12 | 28.3 | 45.2 |
| 7 | 1.5 | 38.5 | 61.6 |
| 8 | 2 | 50.3 | 80.4 |
| 10 | 3.15 | 78.5 | 126 |
| 13 | 5.3 | 133 | 212 |
| 16 | 8 | 201 | 322 |
| 18 | 10 | 254 | 407 |
| 19 | 11.2 | 284 | 454 |
| 20 | 12.5 | 314 | 503 |
| 22 | 15 | 380 | 608 |
| 23 | 16 | 415 | 665 |
| 24 | 18 | 452 | 723 |
| 25 | 20 | 491 | 785 |
| 26 | 21.2 | 531 | 850 |
| 28 | 25 | 616 | 985 |
| 30 | 28 | 706 | 1130 |
| 32 | 31.5 | 804 | 1290 |
| 36 | 40 | 1020 | 1630 |
| 38 | 45 | 1130 | 1810 |
| 40 | 50 | 1260 | 2010 |
| 45 | 63 | 1590 | 2540 |
| 48 | 72 | 1800 | 2890 |
| 50 | 78.5 | 1963 | 3140 |
| oantekeningen: totale úteinlike ferlinging by brekkrêft is min. 20%; | |||
| feroarings fan wurklastlimyt yn relaasje ta temperatuer | |
| Temperatuer (°C) | WLL % |
| -40 oant 200 | 100% |
| 200 oant 300 | 90% |
| 300 oant 400 | 75% |
| mear as 400 | net akseptabel |